DuPont Teijin Films Mylar® OL13AT Polyester Packaging Film, 100 Gauge

 

Subcategory: Polyester, TP; Thermoplastic; Polymer

Key Words: DuPont Packaging Polymers

Material Notes:
Data provided by DuPont Packaging Polymers.

Mylar® OL13AT is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sealable lidding film in packaging refrigerated and frozen foods. Mylar® OL13AT is dual ovenable film which provides very strong, aggressive seals to polar substrates such as amorphous polyester (APET, also PETG), semicrystalline polyester (CPET), polyester coated paperboard, and polyvinylchloride (PVC). Mylar® OL13AT does not seal to polyethylene, polypropylene, or polystyrene. DuPont Teijin Films offers another family of lidding films (RL types) for sealing to these substrates. Mylar® OL13AT is similar to OL12AT but has a thicker seal layer than Mylar® OL12AT to give enhanced seal strength. In general, Mylar® OL13AT can produce non-peeling, near "lock-up" type seals and is recommended for hot fill applications where non-peeling seals are desired. It can also be used in some "post-pasteurized" (steam sterilization) applications where the pressure balance in the package can be properly controlled (via vacuum or overpressure). Mylar® OL13 lidding films have excellent grease and oil resistance.

Mylar® OL13AT lidding films are available with anti-fogging capability to provide better clarity when stored and displayed in refrigerated conditions. This film type is marketed by DuPont Teijin Films as OL13AT and is available with corona treatment on opposite side of film from the heat seal layer.

Available Properties
  • Density
  • Moisture Vapor Transmission
  • Oxygen Transmission
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Secant Modulus
  • Tear Strength Test
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。