DuPont Teflon® PTFE Grade 7B Granular Compression Molding Resin

 

Subcategory: Fluoropolymer; Thermoplastic; PTFE

Key Words: Polytetrafluoroethylene; DuPont Fluoroproducts

Material Notes:
DuPont™ Teflon® PTFE 7B is a white granulated powder with an ultra fine particle size and high bulk density. The ultra-fine particle size minimizes voids even at relatively low molding pressure. Teflon® PTFE 7B is an excellent choice for moldings requiring optimum mechanical and electrical properties. The ultra-fine particle size of Teflon® PTFE 7B promotes good capture and uniform distribution of inorganic fillers when they are added to modify the mechanical properties of moldings. Teflon® PTFE 7B exhibits a mold shrinkage that is intermediate of the mold shrinkage of 7A and 7C grades.

Properly processed products made from neat Teflon® PTFE 7B provide the superior properties typical of the fluoropolymer resins: retention of properties after service at 260°C (500°F), useful properties at –240°C (–400°F), chemical inertness to nearly all industrial chemicals and solvents, and low friction and antistick surfaces. Dielectric properties are outstanding and stable with frequency and temperature. Molded products have moderate stiffness and high ultimate elongation. In a flame situation, products of Teflon® PTFE 7B resist ignition and do not themselves promote flame spread. When ignited by flame from other sources, their contribution of heat is small and with very little smoke.

Statements, or data, regarding behavior in a flame situation are not intended to reflect hazards presented by this or any other material when under actual fire conditions.

Applications

Many end products are molded or fabricated from moldings of Teflon® PTFE 7B—or made with filled compounds based on Teflon® PTFE 7B. The filled compounds provide a wide choice of modified mechanical properties. End products using Teflon® PTFE 7B include skived film and sheet, gaskets, bridge or pipeline bearing pads, piston rings, and diaphragms.

Available Properties
  • Specific Gravity
  • Bulk Density
  • Water Absorption
  • Particle Size
  • Linear Mold Shrinkage
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Flexural Modulus
  • Coefficient of Friction
  • Izod Impact, Notched
  • Volume Resistivity
  • Surface Resistivity per Square
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Arc Resistance
  • Melting Point
  • Flammability, UL94
  • Oxygen Index
  • Drying Temperature
  • 20% Hydrochloric Acid Transmission, g/100sq in.
  • 50% Sodium Hydroxide Transmission, g/100sq in.
  • Acetic Acid Transmission, g/100sq in.
  • Acetone Transmission, g/100sq in.
  • Acetophenone Transmission, g/100sq in.
  • Benzene Transmission, g/100sq in.
  • Carbon Tetrachloride Transmission, g/100sq in.
  • Chemical/Solvent Resistance
  • Detergent Resist. on grit-blasted aluminum, Hours
  • Detergent Resistance on aluminum, Hours
  • Detergent Resistance on grit-blasted steel, Hours
  • Etyl Acetate Transmission, g/100sq in.
  • Folding Endurance, # cycles, .18-.20 mm
  • Heat of Combustion J/g
  • Hexane Transmission, g/100sq in.
  • Piperidine Transmission, g/100sq in.
  • Red Fuming Nirtric Acid Transmission, g/100sq in.
  • Salt Spray Resistance on aluminum, Hours
  • Salt Spray Resistance on steel, Hours
  • Sulfuric Acid Transmission, g/100sq in.
  • Water Transmission, g/100sq in.
  • Weather Resistance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。