DuPont Teflon® PTFE Grade 313A Aqueous Dispersion

 

Subcategory: Fluoropolymer; Thermoplastic; PTFE

Key Words: Polytetrafluoroethylene; DuPont Fluoroproducts

Material Notes:
Teflon® PTFE 313A fluoropolymer resin (formerly called TE-3313) is a negatively charged, hydrophobic colloid, containing approximately 60% (by total weight) of 0.05 to 0.5 mm PTFE (polytetrafluoroethylene) resin particles suspended in water. Seen as a milky white liquid, it also contains approximately 7% (by weight of PTFE) of a nonionic wetting agent and stabilizer. Viscosity at room temperature is approximately 20 cP. Nominal pH is 10.

Compared with other grades of PTFE dispersions, Teflon® PTFE 313A is especially formulated to provide void-free coatings with enhanced surface smoothness and gloss. It imparts many of the unique properties of PTFE resin to porous structures. Teflon® PTFE 313A is similar to Teflon® PTFE 30B. Both are typically used to coat woven glass cloth. Teflon® PTFE 313A offers better gloss and slightly better wetting than Teflon® PTFE 30B.

When properly processed, the PTFE resin in Teflon® PTFE 313A exhibits the superior properties typical of the fluoropolymer resins: retention of properties after service at 260°C (500°F), useful properties at –240°C (–400°F), chemical inertness to nearly all industrial chemicals and solvents, and low friction and antistick surfaces. Dielectric properties are outstanding and stable with frequency and temperature.

Applications

Teflon® PTFE 313A is used for coated glass fabric for high-performance industrial or food conveyor belting and nonadhesive separator sheets for laminating or press blankets requiring high-quality surface finish; electrical insulation for wire, printed circuit boards, and rotating equipment; cast film for capacitors or chemical barriers; and surface coatings for other substrates.

Available Properties
  • Specific Gravity
  • Base Resin Density
  • Solids Content
  • Particle Size
  • pH
  • Viscosity
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。