DuPont Teflon® PFA Grade 345T Extrusion and Molding Resin for High Temperature Applications

 

Subcategory: Fluoropolymer; Thermoplastic; PFA

Key Words: DuPont Fluoroproducts; DuPont PFA

Material Notes:
Teflon® PFA345T us a special-purpose resin available in clear, 2.5mm (0.1in) pellets. This resin is a chemically modified form of Teflon® PFA 345 that combines many of the benefits of the parent resin with several new ones. Like Teflon® PFA345, it offers great flex life and resistance to environmental stress cracking. The additional benefits are improves thermal stability and color while processing.

The improved thermal stability of Teflon® PFA 345T results in reduced amounts of bubbles in final parts and decreased corrosion of processing equipment. This resin can be processed at higher temperatures and higher rated than Teflon® PFA345. Teflon® PFA345T combines the processing ease of conventional thermoplastics with properties similar to those of polytetrafluoroethylene. Properly processed products made from Teflon® PFA345T resin provides the superior properties typical to fluoropolymer resins: retention of physical properties at -196°C (-320°F), and chemical inertness to nearly all industrial chemicals and solvents. Dielectric properties are excellent. Molded products have moderate stiffness and high ultimate elongation.

In a flame situation, products of Teflon® PFA345T resist ignition and no not themselves promote flame spread. When ignited by flame from other sources, the contribution of heat is very small and added at a low rate with very little smoke

Applications

Applications for Teflon® PFA345T include tubing, unsupported pipe linings for production of corrosive chemicals, and wire and cable insulation for chemical environments.

Available Properties
  • Specific Gravity
  • Water Absorption
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Break at Elevated Temperature
  • Flexural Modulus
  • Izod Impact, Notched
  • Volume Resistivity
  • Surface Resistivity per Square
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Arc Resistance
  • CTE, linear 20°C
  • Melting Point
  • Maximum Service Temperature, Air
  • Flammability, UL94
  • Oxygen Index
  • Drying Temperature
  • 20% Hydrochloric Acid Transmission, g/100sq in.
  • 50% Sodium Hydroxide Transmission, g/100sq in.
  • Acetic Acid Transmission, g/100sq in.
  • Acetone Transmission, g/100sq in.
  • Acetophenone Transmission, g/100sq in.
  • Benzene Transmission, g/100sq in.
  • Carbon Tetrachloride Transmission, g/100sq in.
  • Chemical/Solvent Resistance
  • Etyl Acetate Transmission, g/100sq in.
  • Folding Endurance, # cycles, .18-.20 mm
  • Heat of Combustion J/g
  • Hexane Transmission, g/100sq in.
  • Piperidine Transmission, g/100sq in.
  • Red Fuming Nirtric Acid Transmission, g/100sq in.
  • Salt Spray Resistance on aluminum, Hours
  • Sulfuric Acid Transmission, g/100sq in.
  • Water Transmission, g/100sq in.
  • Weather Resistance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。