DuPont Tefzel® HT-2181 Fluoropolymer Resin

 

Subcategory: Fluoropolymer; Thermoplastic; ETFE/ECTFE

Key Words: Ethylene Tetrafluoroethylene Copolymer; DuPont Fluoroproducts

Material Notes:
DuPont™ Tefzel® HT-2181 fluoropolymer resin is a general-purpose resin available in translucent, 2.5-mm (0.1-in) pellets. Compared with other grades of Tefzel® , its most unique features are an intermediate flow rate and a balance of properties that make it suitable for a variety of processes and demanding end uses. Tefzel® HT-2181 and the other Tefzel® fluoropolymers are melt processible, modified copolymers of ethylene and tetrafluoroethylene. They are high-performance resins that can be processed at relatively high rates compared with other fluorocarbon resins. They are mechanically tough and offer an excellent balance of properties.

Tefzel® HT-2181 can perform successfully in applications where other thermoplastics are lacking in mechanical toughness, broad thermal capability, ability to meet difficult environmental conditions, or limited by fabricating problems.

Properly processed products made from neat Tefzel® HT-2181 are inert to most solvents and chemicals, hydrolytically stable, and weather-resistant. The recommended upper service temperature is 155°C (311°F); useful properties are retained at cryogenic ranges. The level and stability of dielectric properties are excellent, and the flame rating is V-0 by the UL94 method. Mechanical properties include outstanding impact strength, cut-through, and abrasion resistance. Statements, or data, regarding behavior in a flame situation are not intended to reflect hazards presented by this or any other material when under actual fire conditions.

Applications

Tefzel® HT-2181 is ideal for many end products, including electrical components, such as sleeving, coil forms, sockets, connectors, and switches; lab ware, such as tubing, valves, containers, and dishes; battery or instrument components that require chemical inertness; chemical service items, such as valve components, seal glands, pipe plugs, and corrugated tubing; and film.

Available Properties
  • Specific Gravity
  • Bulk Density
  • Water Absorption
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Flexural Modulus
  • Izod Impact, Notched
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • Arc Resistance
  • CTE, linear 20°C
  • Melting Point
  • Maximum Service Temperature, Air
  • Flammability, UL94
  • Oxygen Index
  • Chemical/Solvent Resistance
  • Weather Resistance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。