DuPont Tefzel® HT-2185 Fluopropolymer Resin

 

Subcategory: Fluoropolymer; Thermoplastic; ETFE/ECTFE

Key Words: Ethylene Tetrafluoroethylene Copolymer; DuPont Fluoroproducts

Material Notes:
DuPont™ Tefzel® HT-2185 fluoropolymer resin is a special-purpose resin available in translucent, 2.5-mm (0.1-in) pellets. Compared with other grades of Tefzel®, it has a higher flow rate.

Tefzel® HT-2185 and the other Tefzel® fluoropolymers are melt processible, modified copolymers of ethylene and tetrafluoroethylene. They are high-performance resins that can be processed at relatively high rates compared with fluorocarbon resins. They are mechanically tough and offer an excellent balance of properties. Table 1 shows typical property data for Tefzel® HT-2185.

The relatively high flow rate of Tefzel® HT-2185 makes it uniquely suitable for high-speed processing, especially for extruded coatings and injection molding of slender, thin-walled, or intricate shapes. Molded or extruded products made from Tefzel® HT-2185 are preferred for uses that do not involve significant flexural or tensile stress at elevated temperatures. Higher viscosity products such as Tefzel® HT-2181 and Tefzel® HT-2183 are preferred for these applications.

Properly processed products made from neat Tefzel® HT-2185 are inert to most solvents and chemicals, hydrolytically stable, and weather-resistant. The recommended upper service temperature is 150°C (302°F); useful properties are retained at cryogenic ranges. The level and stability of dielectric properties are excellent, and the flame rating is V-0 by the UL94 method. Mechanical properties include outstanding impact strength, cut-through, and abrasion resistance. Statements, or data, regarding behavior in a flame situation are not intended to reflect hazards presented by this or any other material when under actual fire conditions.

Applications

Tefzel® HT-2185 is ideal for many end products, including electrical components, such as sleeving, coil forms, sockets, connectors, and switches; lab ware, such as tubing, valves, containers, and fasteners; battery or instrument components that require chemical inertness; and mechanical parts.

Available Properties
  • Specific Gravity
  • Bulk Density
  • Water Absorption
  • Melt Flow
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Flexural Modulus
  • Izod Impact, Notched
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Melting Point
  • Maximum Service Temperature, Air
  • Flammability, UL94
  • Oxygen Index
  • Chemical/Solvent Resistance
  • Weather Resistance
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。