DuPont™ Bynel® 3126 Adhesive Resin

 

Subcategory: Ethylene Vinyl Acetate; Thermoplastic

Material Notes:
Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins

Applications:Bynel® 3126 adheres to a wide variety of materials. It is most often used to adhere to PE, acid copolymers, and ionomers. The use of Bynel® Series 3100 resins can be advantageous in applications where acid-containing polymers, such as acid copolymers or ionomers, are to be combined with PVDC.

Bynel® Series 3100 resins can be used in coextrusion processes including:

  • blown film
  • cast film/sheet
  • extrusion coating
  • thermal lamination
  • Physical properties Bynel® Series 3100 resins are typical of EVA resins with similar density and melt index values. The rheology characteristics of each grade are different, so one may be better suited than the others for a particular extrusion process.

    Information provided by DuPont™

    Available Properties
    • Density
    • Melt Flow
    • Melting Point
    • Vicat Softening Point
    • Rear Barrel Temperature
    • Middle Barrel Temperature
    • Front Barrel Temperature
    • Adapter Temperature
    • Die Temperature
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。