DuPont™ Trancend™ Extrusion Coating Sealant

 

Subcategory: Ethylene Acrylic Acid; Ionomer; Thermoplastic

Material Notes:
DuPont™ Trancend™ is an ethylene acrylic acid ionomer, expressly designed for extrusion coating, using a new generation of manufacturing technology. This new technology has allowed DuPont to produce a resin of exceptional value, with unique performance characteristics. The resin is designed to run on standard extrusion coating equipment that is designed to process low density polyethylene and standard ethylene copolymers.

Characteristics:

  • Designed as sealant resin capable of unprimed adhesion to aluminum surfaces
  • Heat seal temperatures comparable to DuPont™ Surlyn® 1652 and 9% EAA DuPont™ Nucrel® resins
  • Good hot-tack and seal through contamination performance
  • Cost effective and monolayer and coextruded structures
  • Foil bond durability in the presence of alcohol and oil containing products
  • Information provided by DuPont™

    Available Properties
    • Density
    • Melt Flow
    • Melting Point
    • Vicat Softening Point
    • Rear Barrel Temperature
    • Middle Barrel Temperature
    • Front Barrel Temperature
    • Die Temperature
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。