DuPont Elvax® 3200-2 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating

 

Subcategory: Ethylene Vinyl Acetate; Thermoplastic

Key Words: EVA; DuPont Packaging Polymers

Material Notes:
22.5 wt% Vinyl Acetate.

Elvax® 3200-2 is an extrudable, wax-modified, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.

Additives: Antioxidant.

Applications: Elvax® 3200-2 is designed to provide a low temperature peelable heat seal to itself or many other materials commonly used in flexible packaging applications. The melt properties of this resin allow it to be processed on extrusion coating equipment over a wide range of line speeds and coating thicknesses. It can also be coextrusion coated with a variety of other polymers. Elvax® 200-2 is typically used as a lidding sealant for a variety of formed containers, in replacement of solvent applied heat seal lacquers. It will provide a good seal against HDPE film and sheet, polypropylene film, PVDC, rigid vinyl, rigid and foamed polystyrene, and nitrocellulose coatings.

Information provided by DuPont Packaging Polymers.

Available Properties
  • Density
  • Melt Flow
  • Coefficient of Friction
  • Melting Point
  • Vicat Softening Point
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。