DuPont Nucrel® 30707 Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating

 

Subcategory: Ethylene Acrylic Acid; Thermoplastic; Polymer

Key Words: DuPont Packaging Polymers

Material Notes:
7 wt% Acrylic Acid.

Nucrel® 30707 is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins.

Features/Benefits: Low seal initiation temperature allows high speed packaging. Very good hot tack, seal through contamination, and heat seal strength provides strong, reliable heat seals. Balanced acid content (7% AA) provides good adhesion to both aluminum and low-density polyethylene (LDPE). In film applications, 7 melt flow index (MFI) allows for very good wetting in thermal lamination processes. In extrusion coating applications, 7 MFI provides better performance in internally deckled dies compared to higher MFI extrusion coating resins.

Typical Applications: Cable shield wrap. Sealants for sachets in both food and nonfood applications. Toothpaste tubes, as a foil/LDPE tie layer. Other foil-containing pouches and sachets. Medical/pharmaceutical packaging.

Information provided by DuPont Packaging Polymers.

Available Properties
  • Density
  • Melt Flow
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Secant Modulus, MD
  • Secant Modulus, TD
  • Impact
  • Elmendorf Tear Strength, MD
  • Elmendorf Tear Strength, TD
  • Dart Drop Test
  • Seal Strength
  • Melting Point
  • Vicat Softening Point
  • Haze
  • Gloss
  • Processing Temperature
  • Nozzle Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。