DuPont™ Elvax® 40W Ethylene-Vinyl Acetate Copolymer Resin

 

Subcategory: Ethylene Vinyl Acetate; Thermoplastic

Material Notes:
Elvax® 40W has a higher vinyl acetate content compared with the other Elvax® resins resulting in higher elongation, reduced hardness, improved solubility and adhesion, and significant differences in compatibility. To minimize viscosity changes in hot melt blends during processing, Elvax® 40W also contains butylated hydroxytoluene(BHT). Elvax®40W is supplied in pellet form and to prevent the pellets from blocking, low levels of an amide wax have been added to the polymer.

Typical Applications:

  • Laminating adhesives for a variety of substrates including plastics and films. This grade provides the extended open time often needed in industrial assembly
  • Lacquers for wood, metal, metal foils, paper, and films
  • Fabric and decal coatings
  • Heat-seal coatings for backing card stock used in blister packaging
  • Wood primers and sealers. Combinations of Elvax® 40W and nitrocellulose form the basis for wood sealers offering toughness and good intercoat adhesion
      Elvax® 40W is also suggested for use as a modifier in:
  • Elastomer-based hot melt and hot melt pressure-sensitive adhesion formulations
  • Natural and synthetic elastomers to improve resistance to ozone cracking
  • Caulks and sealants, including those based on asphalt
  • Asphalt road repairing compositions for resurfacing, patching, and crack sealing to improve low temperature flexibility, strength properties, and adhesion
  • Traffic paint formulations
  • Solvent-based and wax-based inks

Information provided by DuPont.

Available Properties
  • Density
  • Viscosity Measurement
  • Vinyl Acetate Content
  • Melt Index of Compound
  • Hardness, Shore A
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Ring & Ball Softening Point
  • Antioxidant
  • Odor
  • Residual VA Monomer, wt%
  • Vinyl Acetate Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。