DuPont Elastomers GLT 505 Formulation

 

Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset

Close Analogs: This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.

Material Notes:
Formulation
Viton® GLT 505100
Zinc Oxide3
N990 Carbon Black30
Diak™ 7 (TAIC)3
Luperox® 101-XL peroxide3

Description: VTR-8525 is a new, developmental 66% fluorine peroxide cured polymer that utilizes DuPont Dow's new Advanced Polymer Architecture technology to create an unique new seal offering for fuel systems. VTR-8525, which will become Viton® GBLT-S once it is fully commercial, has the following attributes:

  • VTR-8525 is a one polymer alternative to GLT and GFLT for fuel seals and fuel injector O-rings
    • Better low temperature sealing than GFLT...–40°C and below
    • Better fuel/alcohol/methanol resistance than GLT
    • Current GFLT and GLT auto specs could be combined into one specification
  • VTR-8525 derives additional benefits from new Advanced Polymer Architecture technology
    • Physical modulus is low, elongation is high - parts are easier to stretch, more tear resistant in automated assembly equipment
    • Cures exceptionally fast to a high state of cure
    • Shows improved mold release/mold fouling properties compared to GLT and GFLT
    • Shows excellent compression set resistance with little (2 hr at 232°C) or no postcure

It is recommended to use at least 70% load factor in an internal mixer. The recommended process aid for VTR-8525 is 0.5 phr of Armeen® 18D. A two part process aid system of Armeen® 18D with Strucktol WS 280 at 0.8 phr each is optimal if that level of process aid can be tolerated in mold shrinkage. The use of Diak™ #8 is NOT recommended as it causes poor mold release and high compression set.

Information provided by manufacturer.

Available Properties
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Modulus of Elasticity
  • 100% Modulus
  • Compression Set, Elevated Temperature
  • Glass Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。