DuPont Elastomers VTR 8605/VTR 8600 Blend

 

Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset

Close Analogs: This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.

Material Notes:
Formulation
VTR 860550
VTR 860050
Zinc Oxide3
N990 Carbon Black30
Diak™ 7 (TAIC)3
Luperox® 101-XL 452

Description: VTR-8605 is a new, 70% fluorine, peroxide-cured, Viton® polymer similar to VTR-8600 but with a significantly lower gum polymer viscosity of ~25 (ML at 121°C). VTR-8605 utilizes revolutionary new Advanced Polymer Architecture technology which includes a new peroxide cure site along with an optimized molecular weight distribution designed to deliver a polymer which:

  • Is ideal for blending with VTR-8600 to reach intermediate viscosity ranges
  • Cures exceptionally fast to a high state of cure
  • Shows improved mold release/mold fouling properties compared to Viton® GF and GF-300
  • Shows improved mold flow and less shear sensitivity than 65 Mooney VTR-8600
  • Shows excellent physical properties with high elongation, both original and aged
  • Shows similar heat, fluids, and low temperature resistance compared to Viton® GF-300
  • Shows improved water resistance/volume swell in water compared to Viton® GF and GF-300
  • Shows excellent compression set resistance with either low or no postcure

VTR-8600 is a new, 70% fluorine peroxide cured polymer similar to Viton® GF but utilizes DuPont Dow's new Advanced Polymer Architecture technology which significantly improves processing and curing characteristics. Advanced Polymer Architecture technology in VTR-8600 upgraded the peroxide cure site along with optimizing the molecular architecture to deliver a polymer which:

  • Cures exceptionally fast to a high state of cure
  • Shows improved mold release/mold fouling properties compared to Viton® GF
  • Shows improved mold flow, less shear sensitivity, and lower extruder die swell for a ~65 Mooney FKM
  • Shows excellent physical properties with high elongation, both original and aged
  • Shows similar heat, fluids, and low temperature resistance compared to Viton® GF
  • Shows excellent compression set resistance with little (2 hr) or no postcure

When mixing VTR-8600 in an internal mixer it is recommended that at least a 70% load factor be used.

Information provided by manufacturer.

Available Properties
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Modulus of Elasticity
  • 100% Modulus
  • Compression Set, Elevated Temperature
  • Glass Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。