DuPont Elastomers VTR 8710 (ETP-600S) Peroxide Cured Fluoroelastomer (FKM) Formulation

 

Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset

Close Analogs: This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.

Material Notes:
Formulation
Viton® Extreme™ ETP-600S100
Zinc Oxide3
N990 Carbon Black30
Diak™ 7 (TAIC)3
Luperox® 101XL453

Description: Viton® Extreme™ ETP-600S (developmental product VTR-8710) is a new specialty fluoroelastomer, built on DuPont Dow's proprietary Advanced Polymer Architecture (APA) technology, that provides the excellent end-use performance of Viton® Extreme™ ETP-900 with significant improvements in processing and cure characteristics. The APA technology upgrades the peroxide cure site and optimizes the molecular structure to deliver a polymer which:

  • Cures faster, and to a higher state of cure, than Viton® Extreme™ ETP-900
  • Provides excellent mold release and low mold fouling
  • Exhibits better mold flow and less shear sensitivity
  • Has improved compression set resistance when compared to ETP-900
  • Gives the same broad fluid and heat resistance of other Viton® Extreme™ ETP polymers

Viton® Extreme™ ETP-600S takes specialty fluoroelastomer performance to a new level of processing ease combined with the excellent end-use performance.

Information provided by manufacturer.

Available Properties
  • Mooney Viscosity
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • 50% Modulus
  • 100% Modulus
  • Compression Set, Elevated Temperature
  • Brittleness Temperature
  • Glass Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。