Dow Engage® 8400 Polyolefin Elastomer

 

Subcategory: Elastomer, TPE; Thermoplastic

Close Analogs: This former DuPont Dow Elastomers product line is now produced by Dow Chemical.

Material Notes:
Description: Engage® 8400 and Engage® 8407 polyolefin elastomers are ethylene-octene copolymers that offer excellent performance in durable injection molded industrial and consumer goods and compression molded gaskets. Engage® 8400 and Engage® 8407 provide high clarity in products requiring visual inspection and allows the use of hot runner molds to enhance production efficiency. In addition, their low density can help control resin and production costs, while reducing the weight of end products. Engage® 8400 and Engage® 8407 also provide good impact properties in blends with polypropylene (PP) and polyethylene (PE), especially in applications requiring high melt flow modifiers. Engage® 8407 is Engage® 8400 with a nominal loose talc coating. The talc is untreated with a 1micron particle size. The product form for Engage® 8400 and Engage® 8407 is free-flowing pellets.

Information provided by manufacturer.

Available Properties
  • Density
  • Melt Index of Compound
  • Hardness, Shore A
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • 2% Secant Modulus
  • Melting Point
  • Vicat Softening Point
  • Comonomer Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。