Dow Engage® 8842 Polyolefin Elastomer

 

Subcategory: Elastomer, TPE; Thermoplastic

Close Analogs: This former DuPont Dow Elastomers product line is now produced by Dow Chemical.

Material Notes:
Description: Engage® 8842 polyolefin elastomer is an ultra-low density ethylene-octene copolymer with a nominal loose talc surface coating. The talc is untreated and has a nominal 1 µm particle size. This product offers the exceptional properties of an ultra-low density elastomer with the added potential of handling this polymer in pellet form. Engage® 8842 has excellent flow characteristics and provides superb impact properties in blends with polypropylene (PP) and polyethylene (PE). It performs well in TPO applications where superior low temperature impact properties are desired. Talc addition significantly improves ability to handle the polymer, but severe blocking can occur if the material is stored under severe conditions (i.e., long duration, elevated temperatures, and/or high weight loadings). To minimize temperature effects, product should be stored at temperatures well below its melting point of 33°C, most preferably below 29°C.

Information provided by manufacturer.

Available Properties
  • Density
  • Mooney Viscosity
  • Melt Index of Compound
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • 2% Secant Modulus
  • Melting Point
  • Brittleness Temperature
  • Comonomer Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。