MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Dow CALIBRE® 300EP 22 Polycarbonate, General Purpose

 

Subcategory: Polycarbonate; Thermoplastic

Key Words: PC

Material Notes:
CALIBRE® 300EP series resins are general purpose polycarbonate resins and can be supplied with a mold release package, a UV stabilizer package or both. CALIBRE 300EP resins exhibit an excellent physical property balance of heat resistance, transparency and impact strength. The CALIBRE 300EP resins have a UL-94 rating of V-2(1). In addition the high melt flow rate allows complex parts to be easily molded.

The CALIBRE 300EP series resins are typically used for appliances, storage media housings, electrical components and lighting.

Available Melt Flow Rate: 22.

Associated products:
CALIBRE 300EP: without a mold release and UV stabilization package
CALIBRE 301EP: including a mold release package
CALIBRE 302EP: including a UV stabilizer package
CALIBRE 303EP: including a mold release and UV stabilizer package.

(1) These numerical flame spread ratings are small scale test values and are not intended to reflect hazards presented by these or any other materials under actual fire conditions.

Ignition resistant chemical additives increase resistance to burning from minor flame sources and permit properly manufactured end products to meet the requirements of certain flammability tests, but resins will burn rapidly under the right conditions of heat and oxygen feed.

Data provided by Dow Chemical.

Available Properties
  • Density
  • Melt Density
  • Water Absorption
  • Moisture Absorption at Equilibrium
  • Linear Mold Shrinkage
  • Melt Flow
  • Hardness, Rockwell R
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Izod Impact, Notched
  • Izod Impact, Unnotched
  • Charpy Impact Unnotched
  • Charpy Impact, Notched, Low Temp
  • Charpy Impact, Unnotched Low Temp
  • Charpy Impact, Notched
  • Tensile Impact Strength
  • Impact Test
  • Electrical Resistivity
  • Dielectric Constant
  • Dielectric Constant, Low Frequency
  • Dielectric Strength
  • Dissipation Factor
  • Dissipation Factor, Low Frequency
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • Flammability, UL94
  • Oxygen Index
  • Haze
  • Transmission, Visible
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。