Dow DOWLEX® 2101 Linear Low Density Polyethylene, Blown Film Grade

 

Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer

Material Notes:
DOWLEX® 2101 Polyethylene resin, a general purpose blown film extrusion resin, is an excellent choice for high speed, thin gauge film applications. It contains medium levels of both slip additive and antiblock additive. It complies with U.S. FDA Regulation 21 CFR 177.1520 (c) 3.2 (a) for food packaging applications. The regulation should be consulted for complete details.

Film properties below based on a film thickness of 25 µm. Data provided by Dow Chemical.

Available Properties
  • Density
  • Thickness
  • Melt Flow
  • Tensile Strength, Ultimate
  • Film Tensile Strength at Yield, MD
  • Film Tensile Strength at Yield, TD
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Tensile Strength, Yield
  • Elongation at Break
  • Elmendorf Tear Strength MD
  • Elmendorf Tear Strength TD
  • Elmendorf Tear Strength, MD
  • Elmendorf Tear Strength, TD
  • Dart Drop
  • Haze
  • Gloss
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。