Dyneon™ 2001 Modified PTFE Paste Extrusion Powder

 

Subcategory: Fluoropolymer; Thermoplastic; PTFE

Key Words: Polytetrafluoroethylene; Dyneon PTFE

Material Notes:
Type I, gr. 2 PTFE. Free flowing powder. Minimum reduction ratio is 20; Max is 1000. Average particle size 500µm.

Dyneon has commercialized a modified PTFE fine powder product for paste extrusion applications. The modified PTFE paste extrusion grade, TFM 2001, combines the traditional attributes of first generation PTFE with benefits such as denser polymer structure and lower permeability; uniform mechanical properties; higher stress cracking resistance; higher pressure resistance under surge stress; and weldability. Dyneon TFM 2001 PTFE is an ideal material for the manufacture of high-performance tubing for hydraulic systems, fuel lines, flexible lines, conveying and transport tubing.

Data provided by Dyneon.

Available Properties
  • Density
  • Apparent Bulk Density
  • Tensile Strength, Ultimate
  • Elongation at Break
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。