Dynasol Calprene® 375 Solution Random SBR

 

Subcategory: Styrene-Butadiene; Elastomer, TS; Thermoset

Material Notes:
Calprene 375 is a Butadiene/Styrene Copolymer, polymerized in solution. It has a random structure with a typical vinyl content of 30%, and is extended with 37.5 phr of naphthenic oil. C-375 is used as ingredient in compounds for battery cases, tires, cables, vulcanized shoe soles and industrial rubber goods. It can replace SBR 1707, 1708, 1778 types. The bales are wrapped in low melting point polyethylene film.

Applications:

  • Tires
  • Footwear
  • Mechanical rubber goods

Compound Test Recipe: ISO-2322 (A)

Information provided by Dynasol.

Available Properties
  • Mooney Viscosity
  • Ash
  • Collected Volatile Condensable Material
  • Tensile Strength at Break
  • Elongation at Break
  • 300% Modulus
  • Hunterlab Color
  • Oil
  • Total Styrene (on polymer)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。