Dynasol Solprene® 416 Thermoplastic Rubber SBS Dry

 

Subcategory: Elastomer, TPE; Styrene-Butadiene; Thermoplastic; Styrenic TPE

Material Notes:
Solprene 416 is a radial styrene/butadiene block copolymer having 30% of styrene content, most of it forming a polystyrenes block which gives the polymer a thermoplastic behavior. It develops properties of vulcanized rubber yet not requiring vulcanization. It is protected with a non staining antioxidant system; FDA approved, suitable for food contact applications and is essentially gel free with a very clear color. Solprene 416 is used as elastomeric modifier for asphalt and plastics, as ingredient of soling formulations and as base for pressure sensitive adhesives. It is available as free flowing porous crumb for easy handling and dissolution, packaged in standard paper bags, super sacs and cardboard boxes.

Applications:

  • Adhesives
  • Plastic modification

Information provided by Dynasol

Available Properties
  • Specific Gravity
  • Volatiles
  • Brookfield Viscosity
  • Viscosity Measure
  • Melt Index of Compound
  • Styrene Content
  • Hardness, Shore A
  • Tensile Strength at Break
  • Elongation at Yield
  • 300% Modulus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。