Dyneon™ Polyetherdiamine HC 1101

 

Subcategory: Polyether; Additive/Filler for Polymer

Material Notes:
Dynamar polyetherdiamine HC 1101 is a linear polyether diprimary amine which contains tetramethylene oxide as the principal recurring unit and has a molecular weight of approximately 10000.

HC 1101 is characterized as follows

  • Primary amine and end group functionally of 2
  • High molecular weight
  • Low toxicity

HC 1101 can be utilized as the flexible reactive segment in block-type copolymer containing both flexible and rigid segments. It may be readily converted into very tough cured elastomers, for instance, by reaction with epoxy resins having an oxirane equivalence greater than one. The reaction mixtures are characteristically liquids which can be poured, cast, or molded and subsequently cured at room temperature, or more rapidly at elevated temperatures. High use levels will form elastomers characterized by the following properties:

  • High tensile strength and elongation
  • Hydrolitic stability
  • Adhesion properties similar to epoxy resins
  • Excellent abrasion resistance
  • High resilience and low heat build-up during dynamic use
  • Wide range of available hardnesses

Information provided by Dyneon, A 3M Company

Available Properties
  • Density
  • Volatiles
  • Viscosity
  • Hardness, Shore A
  • Tensile Strength @ Break
  • Elongation at Break
  • 100% Modulus
  • Rebound
  • Compression Set
  • Melting Point
  • Form
  • Total Amine (meq./gram)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。