Eastman DuraStar DS2000 Polymer, Natural

 

Subcategory: Polyester, TP; Thermoplastic; Polycyclohexylenedimethylene Terephthalate (PCT)

Material Notes:
Durastar DS2000 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2000 has very good toughness as shown by Izod impact resistance. Exposure to aromatic oils often causes crazing or actual fracture of many polymer resins, but DS2000 maintains its physical properties when exposed to these oils, and its appearance is virtually unchanged. Easy to process, it flows readily and fills intricate molds. Under existing United States Food and Drug Administration (FDA) regulations, Durastar DS2000 may be used in food contact articles which comply with the specifications and conditions of use in 21 CFR 177.1240.

Applications/Uses

  • Point of purchase displays
  • Toys/Sporting goods
  • Writing instruments
  • Key Attributes

  • Good chemical resistance
  • Excellent flow
  • Outstanding impact resistance
  • Excellent clarity
  • Fast drying times
  • Quick cycle times

    Available Properties
    • Density
    • Specific Gravity
    • Linear Mold Shrinkage
    • Hardness, Rockwell R
    • Tensile Strength at Break
    • Tensile Strength, Yield
    • Elongation at Break
    • Elongation at Yield
    • Flexural Modulus
    • Flexural Strength
    • Flexural Yield Strength
    • Izod Impact, Notched (ISO)
    • Izod Impact, Unnotched
    • Izod Impact, Notched, Low Temp (ISO)
    • Impact Test
    • Izod Impact, Notched @ -40°C
    • Izod Impact, Unnotched @ -40°C
    • Izod Impact, Notched
    • Deflection Temperature at 0.46 MPa (66 psi)
    • Deflection Temperature at 1.8 MPa (264 psi)
    • Flammability, UL94
    • Haze
    • Transmission, Visible
    • Melt Temperature
    • Mold Temperature
    • Drying Temperature
    • Dry Time
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
  • 请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。