Eastman DuraStar DS1910HF Polymer, Natural

 

Subcategory: Polyester, TP; Thermoplastic; Polycyclohexylenedimethylene Terephthalate (PCT)

Material Notes:
Durastar DS1910HF polymer is a high flow grade of Durastar that contains a mold release. Durastar DS1910HF flow lengths are increased 20-40% relative to Durastar DS1010 as shown by spiral flow testing. Other outstanding features of Durastar are easily maintained such as excellent appearance and clarity, good physical properties, chemical resistance, and easy processing. This high flow product is especially suited for those applications utilizing thin-walled intricate tools. Under existing United States Food and Drug Administration (FDA) regulations, Durastar DS1910HF may be used in food contact articles which comply with the specifications and conditions of use in 21 CFR 177.1240.
This product is certified to ANSI/NSF Standard 51.

Applications/Uses

  • Appliances
  • Furniture/Furniture trim
  • Toys/Sporting goods
  • Floor care
  • Housewares
  • Point of purchase displays
  • Pen/stationary supplies
  • Key Attributes

  • Good chemical resistance
  • Excellent flow
  • Outstanding impact resistance
  • Excellent clarity
  • Fast drying times
  • Quick cycle times

    Available Properties
    • Specific Gravity
    • Water Absorption
    • Linear Mold Shrinkage
    • Hardness, Rockwell R
    • Tensile Strength at Break
    • Tensile Strength, Yield
    • Elongation at Break
    • Elongation at Yield
    • Flexural Modulus
    • Flexural Yield Strength
    • Izod Impact, Unnotched
    • Impact Test
    • Izod Impact, Notched @ -40°C
    • Izod Impact, Unnotched @ -40°C
    • Izod Impact, Notched
    • Deflection Temperature at 0.46 MPa (66 psi)
    • Deflection Temperature at 1.8 MPa (264 psi)
    • Vicat Softening Point
    • Haze
    • Transmission, Visible
    • Melt Temperature
    • Mold Temperature
    • Drying Temperature
    • Dry Time
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
  • 请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。