Eastman Eastalloy MA510 Polymer

 

Subcategory: Polycarbonate; Polyester, TP; Thermoplastic

Material Notes:
Eastalloy MA510 Polymer is a clear copolyester/polycarbonate alloy. It affords the consumer excellent impact strength, chemical resistance, dimensional stability, low shrinkage rates and other enhanced physical properties advantages.

Applications/Uses

  • Medical
  • Medical Devices
  • Key Attributes

  • Good chemical resistance
  • Good Clarity
  • Sterilizable with ethylene oxide, electron beam, and gamma rays
  • Wide range of clear tints and opaque colors
  • Elevated in-use temperature resistance
  • Heat resistance
  • Tough, excellent impact strength

    Available Properties
    • Specific Gravity
    • Water Absorption
    • Linear Mold Shrinkage
    • Tensile Strength at Break
    • Tensile Strength, Yield
    • Elongation at Break
    • Elongation at Yield
    • Flexural Modulus
    • Flexural Strength
    • Izod Impact, Unnotched
    • Impact Test
    • Izod Impact, Notched @ -40°C
    • Izod Impact, Unnotched @ -40°C
    • Izod Impact, Notched
    • Deflection Temperature at 0.46 MPa (66 psi)
    • Deflection Temperature at 1.8 MPa (264 psi)
    • Haze
    • Transmission, Visible
    • Melt Temperature
    • Mold Temperature
    • Drying Temperature
    • Dry Time
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
  • 请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。