Eastman Eastar A150 Copolyester, Film

 

Subcategory: Polyester, TP; Thermoplastic; Polymer

Material Notes:
Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethanol. Eastar A150 is intended primarily for extrusion into film and sheeting for packaging applications. It has excellent hydrolytic stability and good heat stability. Eastar A150 copolyester is lawful for use in food contact applications under food additive regulations published at 21 CFR 177.1240 by the Federal Food and Drug Administration. Therefore, it is lawful for use as a packaging material for meat or poultry foods prepared under federal inspection of the U.S. Department of Agriculture regulations at 9 CFR 318.7 and 381.147.

Applications/Uses

  • Blister Packaging
  • Food Packaging
  • Food-contact applications
  • Rigid Medical
  • Available Properties
    • Density
    • Bulk Density
    • Water Vapor Transmission
    • Oxygen Transmission
    • Carbon Dioxide Transmission
    • Viscosity Measurement
    • Thickness
    • Film Tensile Strength at Yield, MD
    • Film Tensile Strength at Yield, TD
    • Film Tensile Strength at Break, MD
    • Film Tensile Strength at Break, TD
    • Film Elongation at Break, MD
    • Film Elongation at Break, TD
    • Film Elongation at Yield, MD
    • Film Elongation at Yield, TD
    • Tensile Modulus
    • Coefficient of Friction
    • Tear Strength, Total
    • Elmendorf Tear Strength, MD
    • Elmendorf Tear Strength, TD
    • Dart Drop
    • Heat of Fusion
    • Specific Heat Capacity
    • Melting Point
    • Glass Temperature
    • Haze
    • Gloss
    • Transmission, Visible
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。