Eastman Eastar EN001 Copolyester

 

Subcategory: Polyester, TP; Thermoplastic

Material Notes:
Eastar EN001 Copolyester is a thermoplastic polyester copolymer. Eastar EN001 Copolyester has a relatively slow crystallization rate. This broadens the operating window for extrusion and forming processes and helps maintain good clarity when processing much thicker sheet. Eastar EN001 copolyester can also be used for injection molding applications. It is the preferred general-purpose crystallizable PET for thermoforming. Eastar EN001 copolyester is regulated for use in food packaging applications in accordance with US FDA Regulation 21 CFR 177.1315. It is lawful for use under US Department of Agriculture Food Safety Inspection Service regulations as a packaging material for meat or poultry food products prepared under federal inspection.

Applications/Uses

  • Food Packaging
  • Housewares
  • Toys/Sporting goods
  • Writing instruments
  • Available Properties
    • Density
    • Specific Gravity
    • Hardness, Rockwell R
    • Tensile Strength at Break
    • Tensile Strength, Yield
    • Elongation at Break
    • Tensile Modulus
    • Flexural Modulus
    • Flexural Yield Strength
    • Izod Impact, Notched (ISO)
    • Izod Impact, Unnotched
    • Izod Impact, Unnotched (ISO)
    • Izod Impact, Unnotched Low Temp (ISO)
    • Izod Impact, Notched, Low Temp (ISO)
    • Impact Test
    • Izod Impact, Notched @ -40°C
    • Izod Impact, Unnotched @ -40°C
    • Izod Impact, Notched
    • Deflection Temperature at 0.46 MPa (66 psi)
    • Deflection Temperature at 1.8 MPa (264 psi)
    • Haze
    • Transmission, Visible
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。