Eastman EMAC SP2242 Specialty Copolymer

 

Subcategory: Ethylene Methyl Acrylate; Thermoplastic

Material Notes:
EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. For use as heat seal layer, adhesive layer, or modifier for cost/performance enhancement. They are soft, pliable and tough at ambient and freezing temperatures and exhibit excellent ESCR. These polymers exhibit high solids fillability and compatibility with a wide range of polymers. This facilitates their uses as bases for all-purpose concentrates for addition to a wide spectrum of polymers. They process like LDPE.

Applications/Uses

  • Films
  • Available Properties
    • Base Resin Density
    • Methyl Acrylate Content
    • Thickness
    • Base Resin Melt Index
    • Hardness, Shore D
    • Tensile Strength at Break
    • Film Tensile Strength at Break, MD
    • Film Tensile Strength at Break, TD
    • Film Elongation at Break, MD
    • Film Elongation at Break, TD
    • Elongation at Break
    • Secant Modulus, MD
    • Secant Modulus, TD
    • Elmendorf Tear Strength, MD
    • Elmendorf Tear Strength, TD
    • Dart Drop
    • Heat Seal Strength Initiation Temperarture
    • Melting Point
    • Brittleness Temperature
    • Haze
    • Gloss
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。