MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Eastman Neostar FN006 Elastomer

 

Subcategory: Elastomer, TPE; Thermoplastic; Polyester TPE

Material Notes:
Neostar FN006 elastomer is the second in Eastman’s series of tough, clear, durable copolyester ethers. Developed for use in the profile and automotive markets, it can also be used in packaging and tubing applications. Its chemical resistance, flexibility, and toughness make it an ideal choice for applications where strength, durability, and puncture resistance in harsh environments is required. Neostar FN006 can be used in injection molding or cast film, blown film, or tubing extrusion applications. This copolyester has a full range of flexibility and memory without the addition of plasticizers. Considered environmentally preferred due to its non-halogenated material composition, it can be incinerated cleanly without the emission of toxic gases. The target inherent viscosity of this product is 1.6.

Applications/Uses

  • Automotive
  • Flexible hinges
  • Pricing channels
  • Retail pricing fins
  • Driver and passenger side air bags
  • Packaging
  • Profiles
  • Tubing
  • Key Attributes

  • Environmentally preferred, non-halogenated material
  • Excellent chemical resistance
  • Exceptional heat resistance and high temperature dimensional stability
  • High flexibility without plasticizers
  • Solvent bondable
  • Available Properties
    • Specific Gravity
    • Water Absorption
    • Viscosity Measurement
    • Melt Flow
    • Hardness, Shore A
    • Hardness, Shore D
    • Tensile Strength at Break
    • Tensile Strength, Yield
    • Elongation at Break
    • Elongation at Yield
    • Tensile Modulus
    • Flexural Modulus
    • Tear Strength, Total
    • Izod Impact, Notched @ -40°C
    • Heat of Fusion
    • CTE, linear 20°C
    • Specific Heat Capacity
    • Thermal Conductivity
    • Melting Point
    • Crystallization Temperature
    • Vicat Softening Point
    • Brittleness Temperature
    • Glass Temperature
    • Clash Berg Stiffness Temperature
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。