Eastman Tenite 360E461312 Propionate Clear, Trsp

 

Subcategory: Cellulosic; Thermoplastic

Material Notes:
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosic plastics differ with plasticizer levels. Lower plasticizer content yields a harder surface, higher heat resistance, greater rigidity, higher tensile strength, and better dimensional stability. Higher plasticizer content increases impact strength. Tenite cellulosic plastics are available in natural, clear, selected ambers or smoke transparents and black translucent. Color concentrates are available in let-down ratios from 10:1 to 40:1. Tenite Cellulosic Acetate Propionate 360-12 has a plasticizer level of 12%. It is resistant to high temperatures.

Applications/Uses

  • Cosmetics/personal care packaging
  • Medical
  • Pen/stationary supplies
  • Frames
  • Ophthalmic
  • Toothbrushes
  • Key Attributes

  • Ability to be solvent polished, cut, cemented, drilled, and decorated
  • Colorable—color concentrates available
  • High surface gloss
  • Superior primary and secondary fabrication
  • Warm feel
  • Good chemical resistance
  • Excellent clarity
  • Outstanding processability—easy to mold, extrude, or fabricate
  • Tough and durable
  • Available Properties
    • Specific Gravity
    • Water Absorption
    • Linear Mold Shrinkage
    • Collected Volatile Condensable Material
    • Hardness, Rockwell R
    • Tensile Strength at Break
    • Tensile Strength, Yield
    • Elongation at Break
    • Flexural Modulus
    • Flexural Yield Strength
    • Izod Impact, Notched @ -40°C
    • Izod Impact, Notched
    • Volume Resistivity
    • Dielectric Constant
    • Dielectric Strength
    • Dissipation Factor
    • CTE, linear 20°C
    • Specific Heat Capacity
    • Thermal Conductivity
    • Deflection Temperature at 0.46 MPa (66 psi)
    • Deflection Temperature at 1.8 MPa (264 psi)
    • Vicat Softening Point
    • Refractive Index
    • Haze
    • Transmission, Visible
    • Plasticizer, %
    • Soluble Matter Loss, %
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。