Eastman DURASTAR Polymer DS2010 Natural PCTA Copolyester

 

Subcategory: Polyester, TP; Thermoplastic; Polycyclohexylenedimethylene Terephthalate (PCT); Polymer

Key Words: Polycyclohexylenedimethylene Terephthalate

Material Notes:
Product Description: DURASTAR DS2010 polymer contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2010 has very good toughness as shown by Izod impact resistance. Exposure to aromatic oils often causes crazing or actual fracture of many polymer resins, but DS2010 maintains its physical properties when exposed to these oils, and its appearance is virtually unchanged. Easy to process, it flows readily and fills intricate molds. Under existing United States Food and Drug Administration (FDA) regulations, DURASTAR DS2010 may be used in food contact articles which comply with the specifications and conditions of use in 21 CFR 177.1240.

Applications: Floor care; Furniture/Furniture trim; Housewares; Point of purchase displays; Toys/Sporting goods; Writing instruments

Technical Data Sheet

Comments: Properties reported here are typical of average lots. Eastman makes no representation that the material in any particular shipment will conform exactly to the values given.

Information provided by Eastman Chemical.

Available Properties
  • Density
  • Linear Mold Shrinkage
  • Hardness, Rockwell R
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Elongation at Yield
  • Flexural Modulus
  • Flexural Yield Strength
  • Izod Impact, Notched
  • Izod Impact, Notched, Low Temp
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Haze
  • Transmission, Visible
  • Processing Temperature
  • Mold Temperature
  • Drying Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。