Polimeri Europa Koblend PD P 479 Polystyrene-Polyolefin Alloy

 

Subcategory: Polystyrene; Polyolefin; Thermoplastic

Close Analogs: P479

Material Notes:
Special polystyrene alloy for extrusion which combines very high impact strength and excellent chemical resistance to chemicals, oils and fatty foods. Koblend PD P 479 is mainly recommended as monolayer or as coextruded protective layer for refrigerator applications.

Applications: Extrusion of sheets for refrigeration industry as monolayer or coextruded on ESCR-HIPS for the thermoforming of inner liners where HCFC-141b is used as blowing agent for the insulating PU foam.

Koblend PD P 479 satisfies UL94 HB at 1.5 mm (internal test). This grade in natural version complies by composition with the requirements set by the main Regulations for plastic materials intended for food contact (included the EEC Directive 90/128 and following amendments).

Information provided by Polimeri Europa

Available Properties
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。