Equistar Petrothene® GA502022 Linear Low Density Polyethylene

 

Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer; Equistar Linear Low Density Polyethylene; Equistar Polyethylene

Key Words: LLDPE

Material Notes:
Applications
The PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized products offer excellent additive homogeneity, require no transfer equipment modifications and facilitate clean and safe storage and handling. They can be used in either blown or cast film extrusion. GA 502-024 is specifically formulated with extra antioxidant for use in cast film. It contains no other additives.

Processing Techniques
GA 502 series resins exhibit excellent drawdown characteristics. Recommended conditions are 375-425°F melt temperature and a 1.5-3.0:1 blow-up ratio. Using proper techniques, these products can readily be drawn below .5 mil at optimum production rates. Specific recommendations for type of resin and extrusion conditions can be made only when the end use, required properties and processing equipment are known. For further suggestions, please contact your Equistar sales representative.

Certification
GA 502 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520, Subpart C, Item 3.1. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.

Other Information
Blow-Up ratio 2.1:1, Anti-Block level, ppm, High.

Available Properties
  • Density
  • Thickness
  • Melt Flow
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Coefficient of Friction
  • Elmendorf Tear Strength MD
  • Elmendorf Tear Strength TD
  • Dart Drop Test
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • 1% Secant Modulus, MD
  • 1% Secant Modulus, TD
  • Haze
  • Gloss
  • Antiblock
  • Slip Level
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。