Equistar Petrothene® LP540200 High Density Polyethylene

 

Subcategory: Thermoplastic; HDPE; Polymer; Equistar High Density Polyethylene

Key Words: HDPE

Material Notes:
Applications
PETROTHENE LP 5402-00 is a copolymer resin designed for blown film applications. This resin offers high stiffness, excellent appearance and bubble stability and good draw-down. LP 5402-00 is recommended for merchandise bags and multi-wall sack liners and barrier sheeting. It is also useful as a blend component for improved stiffness and machinability.

Certification
LP 5402-00 meets the requirements of the Food and Drug Administration, regulation 21 CFR 177.1520. This regulation allows the use of olefin polymer in “...articles or components of articles intended for use in contact with food.” Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information regarding the suitability of specific products for specific applications.

Processing Techniques
Specific recommendations for processing LP 5402-00 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.
These are typical values and not to be construed as specific product limits.
Data obtained from film produced in a 3½ (89 mm) blown film line, commercials available 8'”(203 mm) die, 415°F (213°C) melt extrusion temperature, 2.5:1 BUR, 1.25 mil

Available Properties
  • Density
  • Water Vapor Transmission
  • Oxygen Transmission
  • Environmental Stress Crack Resistance
  • Thickness
  • Melt Flow
  • Hardness, Shore D
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Tensile Strength @ Yield
  • Tensile Impact
  • Dart Drop Test
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • 1% Secant Modulus, MD
  • 1% Secant Modulus, TD
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  • Brittleness Temperature
  • Melt Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。