Equistar Alathon® M5363 High Density Polyethylene

 

Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer; Equistar High Density Polyethylene; Equistar Polyethylene

Material Notes:
Applications
ALATHON L 4912 is a high molecular weight, high density copolymer with a broad molecular weight distribution. This resin provides excellent stiffness and a good balance of film properties as a single component or in blends. It is designed to process well on grooved feed or smooth bore equipment. L 4912 may be used in a variety of applications such as liners, over-wrap, multi-wall sheeting, merchandise and produce bags.

Certification
L 4912 meets the requirements of the Food and Drug Administration, regulation 21 CFR 177.1520. This regulation allows the use of olefin polymer in “...articles or components of articles intended for use in contact with food.” Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information regarding the suitability of specific products for specific applications.

Processing Techniques
Specific recommendations for processing L 4912 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.

Available Properties
  • Density
  • Melt Flow
  • Spiral Flow
  • Hardness, Shore D
  • Tensile Strength @ Break
  • Tensile Strength @ Yield
  • Elongation at Yield
  • 1% Secant Modulus
  • 2% Secant Modulus
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  • Brittleness Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。