Equistar Petrothene® XL07425 Copolymer

 

Subcategory: Polyolefin; Thermoset; Equistar Wire and Cable Grade

Material Notes:


Applications
PETROTHENE XL07425 is especially formulated for use in flame retardant primary insulation for low voltage automotive wire and cable applications (SAE J1128). Non-discoloring antioxidant and special active peroxide have been added to ensure thermal stability during processing and optimum curing results.

Processing Techniques
XL07425, like other crosslinkable polyolefin compounds, can be extruded as wire and cable insulation by means of a conventional extruder with a continuous vulcanization tube. Below are suggested extrusion and curing conditions for XL07425. These conditions are intended as general guidelines only, and not optimum values, since manufacturing variables such as extruder type and size, continuous vulcanization tube design and cable construction all have an effect on processing crosslinkable compounds. Contact your Equistar sales representative for more information.

Additional Suggestions
Maximum screen pack of 40 mesh
Little or no die land
No predrying normally required
Compression ratio of 2:1-3:1
"Mixing" screw can be used if properly designed to prevent excessive heat build-up
Dies should be cleaned frequently to reduce compound build-up
On-size dies are recommended
Curing line steam temperature should be at least 400°F (205°C)

Physical Properties
All properties determined from compression molded, press cured plaques. The values listed for physical properties are nominal values only and are subject to normal variations consistent with the test methods and/or variations found acceptable to the industry.

Available Properties
  • Density
  • Hardness, Shore D
  • Tensile Strength @ Break
  • Elongation at Break
  • Oxygen Index
  • Feed Temperature
  • Zone 2
  • Zone 3
  • Adapter Temperature
  • Melt Temperature
  • Head Temperature
  • Screw Cooling Temperature
  • Die Cooling Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。