Equistar Petrothene® L3035 Low Density Polyethylene, Film Extrusion Grade

 

Subcategory: Polyethylene; LDPE; Equistar Low Density Polyethylene; Equistar Polyethylene

Material Notes:
Petrothene L3035 is a fractional melt index LDPE resin that exhibits an exceptional balance of optics, modulus, puncture, tear and shrink characteristics. Typical applications include collation shrink film, shrink bundling, pallet shrink film, frozen food packaging, overwraps and heavy duty films where clarity and stiffness are important.

Regulatory Status: The basic resin L3035 meets the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for further information regarding the suitability of specific products for specific applications.

Specific recommendations for the processing of L3035 can be made only when the end use application, required properties and the processing equipment are known. For exact recommendations, please contact your Equistar sales representative.

Available Properties
  • Density
  • Thickness
  • Melt Flow
  • Film Tensile Strength at Yield, MD
  • Film Tensile Strength at Yield, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Impact Test
  • Elmendorf Tear Strength MD
  • Elmendorf Tear Strength TD
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • 1% Secant Modulus, MD
  • 1% Secant Modulus, TD
  • Haze
  • Gloss
  • Melt Temperature
  • Die Opening
  • Blow-up Ratio (BUR)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。