EVAL® EP-J102B Ethylene Vinyl Alcohol Copolymer Resin

 

Subcategory: Ethylene Vinyl Alcohol; Thermoplastic; Polymer

Key Words: EVOH; EVALCA; EVAL Company of America; Ethylene Vinylalcohol

Material Notes:
32 mol % Ethylene.

Data provided by EVALCA. Designed to provide a wide thermoforming range together with high barrier properties. EVAL® EP-J102B is specifically designed for thermoforming applications using polystyrene and polyethylene structural layers. This resin can be used with SPPF or melt phase forming techniques. EVOH is used in packaging applications because of its outstanding gas barrier properties.

Available Properties
  • Density
  • Moisture Vapor Transmission
  • Oxygen Transmission
  • Melt Flow
  • Hardness, Rockwell M
  • Film Tensile Strength at Break, MD
  • Film Elongation at Break, MD
  • Tensile Strength, Yield
  • Modulus of Elasticity
  • Dielectric Constant
  • Dissipation Factor
  • CTE, linear 20°C
  • CTE, linear 100°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  • Glass Temperature
  • Haze
  • Gloss
  • Processing Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。