ExxonMobil Paxon™ HDPE 7004 Crosslinkable Rotational Molding Resin

 

Subcategory: Polyethylene; Thermoplastic; HDPE

Material Notes:
7004 is a UV-stabilized, 35 mesh crosslinkable HDPE powder intended for use in rotational molding. Properly molded parts made with 7004 show exceptional environmental stress cracking resistance, thermal resistance, and notched failure resistance. The high flow base resin promotes rapid melting and outstanding part fill during processing while the finished part exhibits high performance characteristics reflecting crosslinked molecular weight. This resin is available in various colors, plus natural.

Crosslink Potential measured to be 2.5 by ExxonMobil method.

Information provided by ExxonMobil Chemical

Available Properties
  • Bulk Density
  • ESCR 10% Igepal®
  • Tensile Strength @ Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Flexural Modulus
  • Izod Impact, Notched
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  • Brittleness Temperature
  • Features
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。