ExxonMobil Escorene® LD-612 EVA Injection Molding Resin

 

Subcategory: Ethylene Vinyl Acetate; Thermoplastic

Close Analogs: This material is no longer listed in ExxonMobil Chemical's product line.

Key Words: Ethylene Vinyl Acetate; Exxon Chemical Company

Material Notes:
Data provided by the manufacturer, Exxon Chemical.

A 5.8% vinyl acetate copolymer resin designed for molding and extrusion applications requiring low temperatures, flexibility and toughness. This resin can also be considered for blending with homopolymer resins to improve their toughness.

Applications: Large injection molded shapes.

Available Properties
  • Density
  • Environmental Stress Crack Resistance
  • Melt Flow
  • Hardness, Shore D
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Flexural Modulus
  • Tensile Impact Strength
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。