Fibre Glast 88 / 87 General Purpose Epoxy Resin and Hardener

 

Subcategory: Epoxy; Thermoset

Material Notes:
Description:
#88 Epoxy Resin is a 100% reactive low viscosity liquid bisphenol-A based epoxy resin diluted with Alkyl glycidyl ether. This resin is specially designed for applications requiring low viscosity, minimum odor and good color. It is designed to be cured with #87 Epoxy Hardener. #87 Epoxy Hardener is a very reactive modified aliphatic amine edduct, developed for applications where relatively short cure periods at room temperature are required. Compositions based on #88 Epoxy Resin and #87 Epoxy Cure readily at room temperature. The pot life of such compositions is highly dependent on the volume of the mixture, temperature, amount and type of filler loading, and, to a lesser extent, the presence of a reactive diluent.

Properties listed determined on 1/8" thick test specimens at 25°C for 16 hours followed by a pot cure of 2 hours at 100°C.

Applications
Adhesives, decoupage systems, thin-set terrazzo flooring and industrial flooring, epoxy crack injection systems, exposed aggregate wall matrix, wet lay-up laminates, high solids/low VOC high performance architectural coatings.

Information provided by Fibre Glast Developments Corporation.

Available Properties
  • Water Absorption
  • Viscosity
  • Hardness, Shore D
  • Tensile Strength @ Break
  • Elongation at Break
  • Flexural Modulus
  • Flexural Strength
  • Compressive Yield Strength
  • Izod Impact, Notched
  • Volume Resistivity
  • Dielectric Constant
  • Dissipation Factor
  • Maximum Service Temperature, Air
  • Cure Time
  • Pot Life
  • Maximum Exotherm
  • Mix Ratio
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。