Fibre Glast 1101 High-Strength General Purpose Epoxy Adhesive

 

Subcategory: Epoxy; Thermoset

Material Notes:
Description:
#1101 is a light grayish-tan two part epoxy adhesive that was developed especially for difficult bonding problems involving similar or dissimilar materials. #1101 provides excellent adhesion to a wide variety of materials such as aluminum, steel, brass, concrete, brick, glass, stone, ceramics, tile, and wood. #1101 has very good handling characteristics. The mix ratio of 1 to 1 by weight or volume allows for easy measuring. It has a creamy, smooth viscosity. It is very easy to mix, and has good thixotropy for application to contoured or vertical surfaces without sag or runoff. #1101 cures relatively quickly, developing sufficient "green strength" to allow bonded items to be removed from the holding fixtures and handled within a few hours. The cured material has excellent strength as well as good resistance to weak acids, moisture and weather.

Applications
#1101 is an excellent adhesive for all types of bonding applications. It is very versatile, and can bond a wide variety of materials, so it becomes an effective tool in general shop situations. Often #1101 will outperform other supposed high performance materials, and give handling advantages as well. It has been successfully used for many years in a variety of general bonding uses as well as numerous production applications.

Information provided by Fibre Glast Developments Corporation.

Available Properties
  • Density
  • Water Absorption
  • Hardness, Shore D
  • Tensile Strength @ Break
  • Elongation at Break
  • Compressive Yield Strength
  • Shear Strength
  • Cure Time
  • Gel Time
  • Mix Ratio
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。