Fibre Glast 72 White Gel Coat

 

Subcategory: Thermoset

Material Notes:
Description:

#72 is the industry production standard for molding applications. Use as a sandable base coat for painting or polish to a high luster finish. Spray unthinned into molds using a cup gun or blend with Hi-Gloss Additive when performing repairs. Can be tinted with color pigments as needed, changing bold colors into pastels. #72 is a high quality coating developed for use in the fiberglass industry. This gel coat yields a quality finish, with good chemical/water resistance, gloss retention, weatherability, and resiliency. An un-tinted straight white gel coat, #72 is in the color match "C" category, meaning that batch to batch color variation can occur.
#72 White Gel Coat is formulated to meet the rigid requirements of transportation, boating, and sanitary applications. It has enabled customers to meet and surpass all requirements of the American National Standard for plastic bath tubs, shower receptors and shower stalls. ANSI Z 124.1, .2-1995, Sec. 6.1.1.
#72 White Gel Coat is ready to use, easy to spray, sag resistant, fast curing and requires only the addition of the proper amount of #69 Methyl Ethyl Ketone Peroxide to cure.

  • 36% Volatile Organic Compounds
  • Lay up time: 45 - 60 minutes
  • Sag Resistance: Good at 20 mils
  • Complete hide at 8 - 13 mils
  • Color Match CMC maximum DE of 1 unit

Information provided by Fibre Glast Developments Corporation.

Available Properties
  • Brookfield Viscosity
  • Flash Point
  • Gel Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。