Fibre Glast Duratec 1040 Clear Hi-Gloss Gel Coat Additive

 

Subcategory: Polyester, TS; Thermoset

Material Notes:
#1040 can be mixed 1:1 with regular gel coat to reduce viscosity, porosity, and permit a complete open air cure. The reduction in viscosity allows gel coat to be sprayed controllably through siphon and HVLP equipment, reducing sanding and polishing time. Below the waterline repairs still need the addition of #71 Styrene Wax for maximum hardness.

Features:

  • Low Porosity - when used for repairs, blending the additive with gelcoat produces a low porosity surface
  • Reduced orange peel - the low viscosity of the blend results in a smooth finish that is easily sanded
  • Improved properties - for mold surfaces, the blending of the additive with tooling gelcoat creates a higher heat distortion temperature, improved gloss retention, increased impact resistance and reduced subsurface porosity.
  • Superior Finish - when blended one-to-one with gelcoats, the additive created an air-cure enamel-like coating. No air-dry additive is required. When used for gelcoat repair, surfaces are restored to like-new condition.

    Information provided by Fibre Glast Developments Corporation.

    Available Properties
    • Brookfield Viscosity
    • Gel Time
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。