Fibre Glast 1110 CC Vinyl Ester Resin (Casting Properties)

 

Subcategory: Vinyl Ester; Thermoset

Material Notes:
#1110 is a low viscosity, corrosion resistant vinyl ester resin. It is formulated for maximum corrosion resistance to most fuels, vapors, and both acidic and basic chemicals. It is also heat resistant and blended for toughness. The raw materials used in the manufacture of this resin are listed as acceptable in FDA regulatory Title 21 CFR 177.2420 for repeated use in contact with food subject to compliance with the prescribed limitation of that regulation.

Performance:

  • Excellent corrosion resistance
  • Excellent impact strength
  • High tensile elongation
  • FDA application


Properties listed typical cured casting, catalyzed with 1% BPO, cured two hours at 160°F then one hour at 200°F, post cured two hours at 280°F. See also: "Vinyl Ester Resin (Laminate Properties)" for information on that application.

Can be used for hand lay-up and spray-up, filament winding, flake glass and filled lining and coating compounds. Perfect for repairing tank linings, blistering boat hulls, and fabricating tough all-around parts.

Information provided by Fibre Glast Developments Corporation.

Available Properties
  • Density
  • Solids Content
  • Viscosity
  • Hardness, Barcol
  • Tensile Strength @ Break
  • Elongation at Break
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Maximum Service Temperature, Air
  • Flash Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。