Total Finaclear® 530 Clear Impact Polystyrene

 

Subcategory: Polystyrene; Thermoplastic

Close Analogs:

Total Petrochemicals now includes former Fina and Atofina plastics product lines.

Material Notes:
Finaclear® 530 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles, when used in blends with other styrenic polymers such as GPPS. Complemented by inherent reprocessing and recycling capability, Finaclear® 530 is a well established material in both food and non-food transparent packaging applications. Finaclear® 530 complies with most of the food regulations in European countries and with the Food and Drug Administration (FDA) in the USA.

Application

Finaclear® 530 is designed for mono- and multilayer sheet extrusion/thermoforming, cast and blown film extrusion. Due to its specific structure and the well balanced styrene/butadiene ratio, Finaclear® 530 is the material of choice to reach and optimal balance between high impact, good clarity, brilliancy and cost.

Information provided by Total Petrochemicals.

Available Properties
  • Density
  • Bulk Density
  • Melt Index of Compound
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Flexural Modulus
  • Izod Impact, Notched
  • Izod Impact, Notched, Low Temp
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Vicat Softening Point
  • Haze
  • Transmission, Visible
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。