GE Silicones RTV159 High Strength Silicone Adhesive Sealant, Red

 

Subcategory: Silicone; Thermoset; Polymer

Close Analogs:

GE Silicones became a part of Momentive Performance Materials in 2006.

Material Notes:
RTV 159 is a one component, ready-to-use, high strength silicone rubber adhesive sealant. It cures to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature. RTV159 sealant also provides high temperature performance. It releases acetic acid vapors as a by-products of cure.

RTV159 sealant is a paste consistency product which can be applied to horizontal, vertical, and overhead surfaces in applications requiring high strength and temperature performance.

Since this adhesive sealants utilizes a moisture cure system, it must not be used in thicknesses greater than 6mm(1/4in.). Where section depths exceed 6mm (1/4 in.), GE Silicones one-component, addition cure or two-component silicone rubber compounds are suggested.

This sealant was not designed for and should not be used for applications intended for permanent implantation into the human body.

Mechanical properties for specimen cured 3 days at 25°C and 50% relative humidity.

Key Performance Properties:

  • High strength
  • High temperature performance
  • Low temperature flexibility
  • One-component
  • Room temperature cure
  • General primerless adhesion
  • Excellent electrical insulation properties
  • Excellent weatherability, ozone, and chemical resistance

Available Properties
  • Specific Gravity
  • Linear Mold Shrinkage
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Tear Strength
  • Peel Strength
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Brittleness Temperature
  • Dry Time
  • Application rate
  • Color
  • Consistency
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。