Goodfellow Polyethylene naphthalate (PEN) Film

 

Subcategory: Polyester, TP; Thermoplastic; Polymer

Material Notes:
General Description:

A polyester that is chemically quite similar to PET but which is more temperature resistant. So far available only as biaxially oriented and heat stabilized films, they are semi-crystalline and colorless, either crystal clear or slightly hazy (the latter are available from Goodfellow stock). Compared to their PET equivalents, they start to shrink significantly at 190C rather than 150C and are certified for long term electrical use at 155C rather than 105/130C. Their tensile strengths are similar, but the modulus of PEN films is higher - say 25% at ambient temperatures but several times higher in the 100-150C region. They also have better UV resistance and barrier properties and are more resistant to hydrolysis in alkaline or very hot aqueous conditions. They are, however, more expensive and have a lower flex life.

Applications for the films are mainly in the electrical and electronic areas.

Information provided by Goodfellow.

Available Properties
  • Density
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Coefficient of Friction
  • Electrical Resistivity
  • Surface Resistivity per Square
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 20°C
  • Maximum Service Temperature, Air
  • Flammability, UL94
  • Shrinkage
  • Transmission, Visible
  • Chemical Resistance - Alcohols
  • Chemical Resistance - Alkalis
  • Chemical Resistance - Aromatics
  • Chemical Resistance - Concentrated Acids
  • Chemical Resistance - Dilute Acids
  • Chemical Resistance - Greases and Oils
  • Chemical Resistance - Halogens
  • Chemical Resistance - Ketones
  • Permeability to Carbon Dioxide @25°C
  • Permeability to Oxygen @25°C
  • Permeability to Water @25°C
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。