Greene Tweed CHEMRAZ® SD517 Perfluoroelastomer

 

Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset

Material Notes:
Chemraz® SD517, a white-colored perfluoroelastomer, offers the broadest chemical resistance of any elastomer, combining the resilience and sealing force of an elastomer with chemical resitance and lwo extractables similar to PTFE. Providing the lowest temperature sealing properties of any perfluoroelastomer on the market (-22°F, -30°C), Chemraz SD517 is an ideal seal component for sub-ambient mechanical seal applications and is the preferred alternative to encapsulated O-rings. With its white color, Chemraz SD517 meets the needs of applications requiring non-black elastomers.

Chemraz SD517’s many features make it well suited for critical applications and difficult seal replacement locations where maximizing MTBR (mean time between replacement) is paramount.

Chemraz components are available for use as O-rings, gaskets, sanitary seals and many other custom shapes.

This product is FDA and USP Class VI compliant making it an ideal product for electrometric applications requiring regulatory compliance.

Applications:Mechanical seals

  • Valves
  • Pumps
  • Mixers
  • Fermenters
  • Biomedical equipment
  • Couplings

    Information provided by Green Tweed

    Available Properties
    • Specific Gravity
    • Hardness, Shore A
    • Tensile Strength @ Break
    • Tensile Modulus
    • Compression Set
    • Maximum Service Temperature, Air
    • Minimum Service Temperature, Air
    • Color
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
  • 请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。