Greene Tweed FLUORAZ® 890 Fluoroelastomer, FEPM

 

Subcategory: Fluoropolymer, TS; Elastomer, TS; Thermoset

Material Notes:
Sanitary gaskets made from Fluoraz® 890 are ideal for use in standard SIP and CIP applications where EPDMs and FKMs fail. While EDPMs and FKMs can provide a deal for extended periods, changes in physical properties can have adverse effects beyond simple volume swell. A decrease in hardness or drop in modulus signals a reduction in compressive strength. If a sanitary gasket is retorqued to the installations specification, the gasket will be compressed at a greater level than desired, resulting in increased intrusion into the process stream. An increase in hardness/modulus and a drop in elongation means embrittlement. The seal will be undertorqued, resulting in either leaks or cracking.

Fluoraz 890 is formulated for use in sanitary gaskets where both USP and FDA compliance is required, making it an excellent compound for both pharmaceutical and other hygienic fluid handling applications such as seals for brewery applications. Fluoraz 890 metal and TOC extractables are an order of magnitude lower than premium competitive FKM formulations, ensuring little or no contamination into the process stream. Fluoraz 890 also meets the extractive requirements of both 21 CFR 177.2600 (e), (f) and 21 CFR 177.2400 (d) extraction testing for perfluoroelastomers. Fluoraz 890 sanitary gaskets by Green Tweed are designed for minimal intrusion.

Fluoraz 890 is also available in O-rings and custom shapes where a medium durometer hardness is desired.

Information provided by Green Tweed

Available Properties
  • Specific Gravity
  • Hardness, Shore A
  • Tensile Strength @ Break
  • Elongation at Break
  • Tensile Modulus
  • Compression Set
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Color
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。